LabCore Materials
Battery Separator Discs for Coin Cell Research | PP/PE, 16-20μm
Pre-cut PP/PE separator discs for Li-ion & Na-ion coin cell research: 16.2-19 mm dia, 16-20 μm thick, 100 pcs/pack. Prevents electrode shorts while allowing ion transport.

Pre-cut separator discs for coin cell assembly, cut to size and ready to use in CR20xx and other coin cell research configurations.Designed for lithium-ion and sodium-ion battery research: the disc separates the cathode and anode to prevent short-circuiting while allowing ion migration through its porous structure.
Available options (100 pcs per box):
Φ19 mm × 20 μm PE
Φ19 mm × 16 μm PP
Φ16.2 mm × 16 μm PP
Key parameters (Φ19 mm × 16 μm PP): porosity 35±4%, air permeability 310±50 s/100ml, puncture strength ≥220 g, tensile strength MD ≥1200 kg/cm² (TD ≥100 kg/cm²), shrinkage at 120°C/1h ≤0.5% (TD) / ≤8.0% (MD).
Usage: place one separator disc between the anode and cathode inside the coin cell, add electrolyte, then seal with the cell crimper.
Dry film, ships as empty consumable — no electrolyte, no lithium, not classified as dangerous goods.
Order / Quote
| Model | Pack | Price | Action |
|---|---|---|---|
| 162MM-16UM-PP-100PCSMade to orderShips in 5 business days | Φ16.2mm-16μm-PP-100pcs | $41.00 | |
| 19MM-16UM-PP-100PCSMade to orderShips in 5 business days | Φ19mm-16μm-PP-100pcs | $42.00 | |
| 19MM-20UM-PE-100PCSMade to orderShips in 5 business days | Φ19mm-20μm-PE-100pcs | $45.00 |
Specifications
| Parameter | Value | Unit |
|---|---|---|
| Material | PP/PE | N/A |
| Diameter | Φ19 / Φ16.2 | mm |
Cut to size and ready to use in CR20xx and other coin cell research configurations
Product Images

Shipping & Compliance
- Non-Amazon orders ship from our Shenzhen facility via DHL / FedEx — typically 5–10 business days in transit to the US and EU, with tracking. Bulk orders may go by air freight.