极耳套装
铝极耳与镍极耳成对配套,附宽度精准匹配的密封胶带。提供 5 mm 与 8 mm 两种宽度。

High-purity nickel battery tabs with polyimide tape insulation. 5mm and 8mm widths available. Essential for pouch cell electrode connections. Ships worldwide.
Battery tabs (also called electrode tabs or current leads) are the metallic strips that
connect the electrode inside a pouch cell to external circuitry. Our tabs feature 99.6%
pure nickel for aluminum-clad cells or pure aluminum for nickel-clad cells, with
polyimide tape for electrical insulation.
📖 Related Guide: Battery Tab Selection Guide
订购 / 询价
| 型号 | 包装 | 价格 | 操作 |
|---|---|---|---|
| TAB-5-10现货 · Amazon | 极耳套装 5 mm,10 对铝极耳 10 片 + 镍极耳 10 片,宽 5 mm,附 0.5 cm 胶带 1 卷 | $20.00 | 在 Amazon 购买 1+ 件可询批发报价 → |
| TAB-5-20现货 · Amazon | 极耳套装 5 mm,20 对铝极耳 20 片 + 镍极耳 20 片,宽 5 mm,附 0.5 cm 胶带 1 卷 | $30.00 | 在 Amazon 购买 1+ 件可询批发报价 → |
| TAB-8-10现货 · Amazon | 极耳套装 8 mm,10 对铝极耳 10 片 + 镍极耳 10 片,宽 8 mm,附 0.8 cm 胶带 1 卷 | $20.00 | 在 Amazon 购买 1+ 件可询批发报价 → |
| TAB-8-20现货 · Amazon | 极耳套装 8 mm,20 对铝极耳 20 片 + 镍极耳 20 片,宽 8 mm,附 0.8 cm 胶带 1 卷 | $30.00 | 在 Amazon 购买 1+ 件可询批发报价 → |
技术规格
| 参数 | 数值 | 单位 |
|---|---|---|
| 极耳宽度 | 5 / 8 | mm |
| 材质 | Aluminum (cathode) + Nickel (anode) | |
| 纯度 | 99.6 (Ni tab) | % |
| 绝缘 | Polyimide tape | |
| 配套方式 | Matched pairs, Al + Ni | |
| 密封胶带 | 1 roll included per pack, width matched to tab |
胶带宽度与极耳宽度精准匹配:5 mm 极耳配 0.5 cm 胶带,8 mm 极耳配 0.8 cm 胶带。不含焊料。
产品图片

运输与合规
- 非 Amazon 订单由深圳仓经 DHL / FedEx 直发,欧美通常 5–10 个工作日送达,全程可追踪。大批量可走空运。
- 以空壳硬件出货,不含电解液与锂,非危险品。